In the first in a series of FESI Publishing Monographs, Peter M Scott reflects on almost 50 years working on materials ageing and countermeasures in light water reactors (LWRs), first as a researcher with the UK Atomic Energy Authority, then later as a senior materials specialist with the French nuclear steam supply system (NSSS) vendor Framatome, and finally as an independent consultant.

Preface

Chapter 1
Introduction
1.1 Light Water Reactor Basic Designs
1.2 Materials
1.3 Water Chemistry, Radiolysis, and Corrosion Basics

Chapter 2
Stress Corrosion Cracking in Carbon and Low-Alloy Steels

Chapter 3
Stress Corrosion Cracking in Stainless Steels
3.1 Effects of Impurity Contamination
3.2 Boiling Water Reactor Experience with No Neutron Irradiation Effects
3.3 Pressurised Water Reactor Experience with No Neutron Irradiation effects
3.4 Neutron Irradiation Effects

Chapter 4
Stress Corrosion Cracking in Nickel-Base Alloys
4.1 Boiling Water Reactor Experience
4.2 Pressurised Water Reactor Experience

Chapter 5
High-Strength Alloys

Chapter 6
Proactive Materials Degradation Assessment